![](https://potus31.com/wp-content/uploads/2021/04/hammered_bronzclay.jpg)
Tried to hammer this one out with the ball peen then the planishing hammer. Ended up flat as a penny and could have gone thinner. Seems sintering leaves lots of space between particles.
319/365
Tried to hammer this one out with the ball peen then the planishing hammer. Ended up flat as a penny and could have gone thinner. Seems sintering leaves lots of space between particles.
319/365
But very nice!